Alpha Knife Supply has started selling a new steel, 26C3. It is not stainless. It is not powder metallurgy. It won't be known for extreme toughness. It won't be known for extreme wear resistance. It will be known, if properly ground and heat treated, for extreme edge stability. The steel recipe is very similar to infamous Hitachi White:
C: 1.25%
Cr: 0.3
Mn: 0.38
That is it. First batch went on sale today at noon, sold out by 5PM. As quenched hardness Rc67-68. Will be interesting to see how it works.
scott

scott
[www.etsy.com]
Re: New old steel 26C3
May 11, 2019 06:31AM
That looks like a nice steel to use.

---------------------------------------------------------
Stone Sharp Edges
[www.youtube.com] [www.facebook.com] [www.instagram.com]

"I am still discussing issues of steels and performance at this stage.

-Cliff"

"Roman Landes said:
Cause geometry cuts, .....steel determines the level and the duration"

Sal Glesser -
".But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of "designing in the dark"...

sal"