Alpha Knife Supply has started selling a new steel, 26C3. It is not stainless. It is not powder metallurgy. It won't be known for extreme toughness. It won't be known for extreme wear resistance. It will be known, if properly ground and heat treated, for extreme edge stability. The steel recipe is very similar to infamous Hitachi White:
C: 1.25%
Cr: 0.3
Mn: 0.38
That is it. First batch went on sale today at noon, sold out by 5PM. As quenched hardness Rc67-68. Will be interesting to see how it works.
scott

scott
[www.etsy.com]
Re: New old steel 26C3
May 11, 2019 06:31AM
That looks like a nice steel to use.

___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
me2
Re: New old steel 26C3
July 22, 2020 03:17AM
Is this stuff still out there or have people poo poo-ed it away? It doesnt tick any of the boxes so I just figure it will be gone after the initial batch.
Re: New old steel 26C3
July 26, 2020 12:09PM
The is only one maker that I know of that uses it [www.isasmedjan.com]
Re: New old steel 26C3
July 28, 2020 12:31PM
Speak of the devil :

[www.youtube.com]

-uses this steel as the core
Sorry, only registered users may post in this forum.

Click here to login