March 20, 2019 08:49PM




------------------------------------------------------------------------------------------------------------------------------------------------------
"Gotta love living in 2019 baby, (63rc too soft on a production knife)"
--Shawn Houston

"I am still discussing issues of steels and performance at this stage."
--Cliff Stamp

"Cause geometry cuts, .....steel determines the level and the duration"
--Roman Landes

"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' "
--Sal Glesser
------------------------------------------------------------------------------------------------------------------------------------------------------
StoneSharpEdges
Re: Things that are actually ok - sharpening videos
June 29, 2019 11:42AM




------------------------------------------------------------------------------------------------------------------------------------------------------
"Gotta love living in 2019 baby, (63rc too soft on a production knife)"
--Shawn Houston

"I am still discussing issues of steels and performance at this stage."
--Cliff Stamp

"Cause geometry cuts, .....steel determines the level and the duration"
--Roman Landes

"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' "
--Sal Glesser
------------------------------------------------------------------------------------------------------------------------------------------------------
StoneSharpEdges
Re: Things that are actually ok - sharpening videos
July 03, 2019 03:05PM




------------------------------------------------------------------------------------------------------------------------------------------------------
"Gotta love living in 2019 baby, (63rc too soft on a production knife)"
--Shawn Houston

"I am still discussing issues of steels and performance at this stage."
--Cliff Stamp

"Cause geometry cuts, .....steel determines the level and the duration"
--Roman Landes

"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' "
--Sal Glesser
------------------------------------------------------------------------------------------------------------------------------------------------------
StoneSharpEdges
Re: Things that are actually ok - sharpening videos
July 30, 2019 11:13AM
[www.youtube.com]




------------------------------------------------------------------------------------------------------------------------------------------------------
"Gotta love living in 2019 baby, (63rc too soft on a production knife)"
--Shawn Houston

"I am still discussing issues of steels and performance at this stage."
--Cliff Stamp

"Cause geometry cuts, .....steel determines the level and the duration"
--Roman Landes

"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' "
--Sal Glesser
------------------------------------------------------------------------------------------------------------------------------------------------------
StoneSharpEdges
Re: Things that are actually ok - sharpening videos
August 05, 2019 06:55PM
Rough Rooster Knife Sharpening Spyderco ZDP 189 Hair Whittling Off Arkansas Stones:
[www.youtube.com]




------------------------------------------------------------------------------------------------------------------------------------------------------
"Gotta love living in 2019 baby, (63rc too soft on a production knife)"
--Shawn Houston

"I am still discussing issues of steels and performance at this stage."
--Cliff Stamp

"Cause geometry cuts, .....steel determines the level and the duration"
--Roman Landes

"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' "
--Sal Glesser
------------------------------------------------------------------------------------------------------------------------------------------------------
StoneSharpEdges
Re: Things that are actually ok - sharpening videos
October 29, 2019 07:54PM
[www.youtube.com]




------------------------------------------------------------------------------------------------------------------------------------------------------
"Gotta love living in 2019 baby, (63rc too soft on a production knife)"
--Shawn Houston

"I am still discussing issues of steels and performance at this stage."
--Cliff Stamp

"Cause geometry cuts, .....steel determines the level and the duration"
--Roman Landes

"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' "
--Sal Glesser
------------------------------------------------------------------------------------------------------------------------------------------------------
StoneSharpEdges
JDW
Re: Things that are actually ok - sharpening videos
October 30, 2019 12:22AM
Some good points there! I use the same hone for shaping edges. Then I usually finish and maintain them with my Fallkniven DC4 diamonds side. (pocket knives). Works well for me! :-)
Re: Things that are actually ok - sharpening videos
November 18, 2019 02:30PM
Here is the new JavaScript app with Larrin Thomas' formula to estimate CATRA TCC. The new info for S45VN is there also:

[drive.google.com]


PS: Thank you to Larrin Thomas for letting me use his formula, and to ShaperAndMower who re-wrote and helped me write my original JavieraScript program and helped me a lot with me C++ version. Just download the app and put the file location in the address bar and it will run in your browser. If you have any issues just contact me. Please share this with all your friends. Thank you everyone for the support and giving me a rewarding experience to do projects like this. If you have any suggestions or ideas about features or improvements please contact me.

------------------------------------------------------------------------------------------------------------------------------------------------------
"Gotta love living in 2019 baby, (63rc too soft on a production knife)"
--Shawn Houston

"I am still discussing issues of steels and performance at this stage."
--Cliff Stamp

"Cause geometry cuts, .....steel determines the level and the duration"
--Roman Landes

"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' "
--Sal Glesser
------------------------------------------------------------------------------------------------------------------------------------------------------
StoneSharpEdges
Re: Things that are actually ok - sharpening videos
December 17, 2019 12:17AM
[www.youtube.com];




------------------------------------------------------------------------------------------------------------------------------------------------------
"Gotta love living in 2019 baby, (63rc too soft on a production knife)"
--Shawn Houston

"I am still discussing issues of steels and performance at this stage."
--Cliff Stamp

"Cause geometry cuts, .....steel determines the level and the duration"
--Roman Landes

"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' "
--Sal Glesser
------------------------------------------------------------------------------------------------------------------------------------------------------
StoneSharpEdges
Re: Things that are actually ok - sharpening videos
December 25, 2019 10:01AM
[www.youtube.com]




------------------------------------------------------------------------------------------------------------------------------------------------------
"Gotta love living in 2019 baby, (63rc too soft on a production knife)"
--Shawn Houston

"I am still discussing issues of steels and performance at this stage."
--Cliff Stamp

"Cause geometry cuts, .....steel determines the level and the duration"
--Roman Landes

"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' "
--Sal Glesser
------------------------------------------------------------------------------------------------------------------------------------------------------
StoneSharpEdges
Re: Things that are actually ok - sharpening videos
December 27, 2019 02:33PM
[www.youtube.com]




------------------------------------------------------------------------------------------------------------------------------------------------------
"Gotta love living in 2019 baby, (63rc too soft on a production knife)"
--Shawn Houston

"I am still discussing issues of steels and performance at this stage."
--Cliff Stamp

"Cause geometry cuts, .....steel determines the level and the duration"
--Roman Landes

"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' "
--Sal Glesser
------------------------------------------------------------------------------------------------------------------------------------------------------
StoneSharpEdges
Sorry, only registered users may post in this forum.

Click here to login