Posted by CliffStamp 
Re: Things that are actually ok - sharpening videos
March 20, 2019 08:49PM




___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
Re: Things that are actually ok - sharpening videos
June 29, 2019 11:42AM




___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
Re: Things that are actually ok - sharpening videos
July 03, 2019 03:05PM




___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
Re: Things that are actually ok - sharpening videos
July 30, 2019 11:13AM
[www.youtube.com]




___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
Re: Things that are actually ok - sharpening videos
August 05, 2019 06:55PM
Rough Rooster Knife Sharpening Spyderco ZDP 189 Hair Whittling Off Arkansas Stones:
[www.youtube.com]




___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
Re: Things that are actually ok - sharpening videos
October 29, 2019 07:54PM
[www.youtube.com]




___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
JDW
Re: Things that are actually ok - sharpening videos
October 30, 2019 12:22AM
Some good points there! I use the same hone for shaping edges. Then I usually finish and maintain them with my Fallkniven DC4 diamonds side. (pocket knives). Works well for me! :-)
Re: Things that are actually ok - sharpening videos
November 18, 2019 02:30PM
Here is the new JavaScript app with Larrin Thomas' formula to estimate CATRA TCC. The new info for S45VN is there also:

[drive.google.com]


PS: Thank you to Larrin Thomas for letting me use his formula, and to ShaperAndMower who re-wrote and helped me write my original JavieraScript program and helped me a lot with me C++ version. Just download the app and put the file location in the address bar and it will run in your browser. If you have any issues just contact me. Please share this with all your friends. Thank you everyone for the support and giving me a rewarding experience to do projects like this. If you have any suggestions or ideas about features or improvements please contact me.

___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
Re: Things that are actually ok - sharpening videos
December 17, 2019 12:17AM
[www.youtube.com];




___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
Re: Things that are actually ok - sharpening videos
December 25, 2019 10:01AM
[www.youtube.com]




___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
Re: Things that are actually ok - sharpening videos
December 27, 2019 02:33PM
[www.youtube.com]




___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
Re: Things that are actually ok - sharpening videos
January 19, 2020 09:34AM
[www.youtube.com]





___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
Re: Things that are actually ok - sharpening videos
January 28, 2020 11:11PM
[www.youtube.com]




___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
cKc
Re: Things that are actually ok - sharpening videos
March 24, 2020 09:10AM
Quote
jasonstone20
[www.youtube.com]


you know.. this is something that i still literally cannot comprehend..

52 minutes sharpening a knife..
often, the people that love the stones, and sharpen for hours on end maybe do it for enjoyment,
but for the price of just one fancy stone, you can buy a 1x30 grinder, or go up a little to a 2x48 and use a 120 grit belt to thin the primary bevel quickly and safely in a couple minutes, and then take it to the stones to clean up and do the edge.

anyone that can learn that level of control on a stone, will not have an issue using a tiny grinder.

----------------------------------------------------------------------
It's not Cliff, its Dr Stamp
#kebabstickcut, it's a thing - make it happen
Re: Things that are actually ok - sharpening videos
March 28, 2020 11:43AM
What you said about the 1x30 vs an expensive stone makes sense. I’ve got an Imacasa machete and two heavy/thick Condor machetes that are in desperate need of a regrind and or more.

Especially the Imacasa machete, it’s essentially unfinished but the design is fantastic for brush and small trees. Balance point is about 3” or 4” in front of the handle, full distal taper, solid handle shape, good 1075 steel. I just have no way to make it functional without a 1x30 or similar tool.

But for smaller knives it can also pay to have something like the Shapton Pro 120 around, that’s a safe way to do full zero grinds on folders and such from the kitchen or living room, not really possible with the grinders.

I think a 1x30, the Shapton 120, and a new diamond finishing stone (a DMT or Atoma 600) are really all I have need for right now. Those and maybe a new set of wood rasps and a couple good quality steel files.
Re: Things that are actually ok - sharpening videos
March 28, 2020 12:49PM
I really would like to get a belt sander, like a Harbor Freight 1x30 for gross metal removal, but I live in a small one bedroom apartment (less than 1000 sq'). There is a Shop Co-Op right across the street that has all the equipment for knife making, I plan one day to join it.

___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
cKc
Re: Things that are actually ok - sharpening videos
March 31, 2020 05:46AM
I understand that living in a small apartment excludes the use of a grinder, and that makes sense. but i think many of the people with these big knives etc probably don't have those limitations. maybe they do..

Joining the co-op shop is probably a good idea, get into it grinning smiley

you make me laugh saying you are in a small less than 1000sft apartment.. in most of the world, 1000sft is a 3 bedroom apartment.
I'm in a 2bedfroom apartment considered roomy at 538s ft

tell me it's less than 100 and that was a typo and I'll start sympathizing grinning smiley grinning smiley

i do have thoughts for people in apartments though.. buy the 1x30 chassis.. go find an old broke one for $20, and replace the motor with an electric drill on slow speed and now you have something where you will have a heck of a lot more control than a stone.. almost relaxing grinning smiley, and quiet, and not messy if its at a speed of only 50rpm

----------------------------------------------------------------------
It's not Cliff, its Dr Stamp
#kebabstickcut, it's a thing - make it happen
Re: Things that are actually ok - sharpening videos
March 31, 2020 10:46AM
cKc,
I just looked it up, my apartment is 540' sq ft:



___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
cKc
Re: Things that are actually ok - sharpening videos
April 02, 2020 08:00AM
thats not a bad size grinning smiley slightly bigger than mine. we have 4 people squeezed in right now. lol.


I have another idea for apartments and using stones grinning smiley

1. and old turntable record player and velcro sandpaper grinning smiley
2. some device that holds a stone and rocks back and forward at adjustable speed while holding the knife still grinning smiley

----------------------------------------------------------------------
It's not Cliff, its Dr Stamp
#kebabstickcut, it's a thing - make it happen
Re: Things that are actually ok - sharpening videos
April 02, 2020 12:08PM
cKc,
Ha! I have a few bicycles, I could get a grind wheel and run it off the bike.

It is just me and my old lady on my apartment, so it isn't that cramped. I can see how 4 people would be tight quarters.

___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
cKc
Re: Things that are actually ok - sharpening videos
April 02, 2020 01:29PM
In that case.. get a 1 x 30 and attach a crank handle.. while watching tv, have her turn the handle and you sharpen grinning smiley, quiet, slow, and a team game grinning smiley

----------------------------------------------------------------------
It's not Cliff, its Dr Stamp
#kebabstickcut, it's a thing - make it happen
Re: Things that are actually ok - sharpening videos
June 14, 2020 05:09PM
[www.youtube.com]




Well, I saw shiny, I didn't see sharp.

___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
Re: Things that are actually ok - sharpening videos
June 15, 2020 02:39AM
Quote
jasonstone20
Well, I saw shiny, I didn't see sharp.

Because you have too little experience from real use and sharpening
and know nothing about obvious "shiny-sharp"..

You see the shine to reflect in your eyes.. doubts are "shined" away..

www.instagram.com/jscuttingtools
Re: Things that are actually ok - sharpening videos
June 15, 2020 05:02AM
JSCT,
Hahaha.

___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
Re: Things that are actually ok - sharpening videos
July 16, 2020 09:35AM
Power serrated sharpening :

[www.youtube.com]

-short video
-very detailed analysis of how to handle different serration patterns with specialized tools
-focus on raise a burr, grind it off
-no sharpness demonstration, but likely solid
Re: Things that are actually ok - sharpening videos
July 18, 2020 10:28PM
[www.youtube.com]

big knife small hand held soft ark - not a bad idea for touch and go if you are a line cook

-------------------------------------------------------------------------------------------------------------

Life is GOOD!

[www.youtube.com]
Re: Things that are actually ok - sharpening videos
September 14, 2020 09:02PM
Cool sharpening trick from Neeves Knives that I saw Jef Jewell post about on Stefan_Wolf's YouTube channel. I was wondering what Jef was talking about, since the description he gave wasn't making sense to me, as I couldn't envision it (Not Jef's fault). Anyway, here is the trick: You put the knife on the stone, and were your index finger is indented, you highlight that with a sharpie marker. You then pinch your fingers together, to transfer the mark to your thumb. Then you highlight the transfer mark with the marker on your thumb. You now have a guide on both directions were to place the blade for a consistent angle:

[www.youtube.com]




___________________________________________________________________________________________
"Gotta love living in 2019 baby, (63rc too soft on a production knife)" -- Shawn Houston
"But can it cut a bamboo skewer?" -- Kyley Harris
"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp
"Cause geometry cuts, .....steel determines the level and the duration" -- Roman Landes
"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' " -- Sal Glesser
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals
cKc
Re: Things that are actually ok - sharpening videos
October 12, 2020 08:57AM
Quote
jasonstone20
Cool sharpening trick from Neeves Knives that I saw Jef Jewell post about on Stefan_Wolf's YouTube channel. I was wondering what Jef was talking about, since the description he gave wasn't making sense to me, as I couldn't envision it (Not Jef's fault). Anyway, here is the trick: You put the knife on the stone, and were your index finger is indented, you highlight that with a sharpie marker. You then pinch your fingers together, to transfer the mark to your thumb. Then you highlight the transfer mark with the marker on your thumb. You now have a guide on both directions were to place the blade for a consistent angle:

[www.youtube.com]


Its like never removing the training wheels from your bicycle.. and interestingly, training wheels tend to have a negative effect on learning speed. the more you hinder your bodies innate abilities to guage and measure and hold things steady, the harder it is to do it without the gimmicks.

i think my skin is far too sensitive to want to sit there rubbing my skin off on abrasives like that. there is also the fact that i dont think you could do that technique at speed, so you are either going to bleed, or go very very slow.

as you progress through it, its clear as he goes a bit faster that his thumb is not perpendicular as it was when making the mark, and also not really touching the stone, but floating above. once you weigh all these things in, its prob not more than 1-2 degrees accurate, which is no different than holding freehand anyway for most people. you might as well just tape a couple of teflon wedges onto each side of the blade if going down this route.

But hey. if he gets the knife sharp.. thats what counts

----------------------------------------------------------------------
It's not Cliff, its Dr Stamp
#kebabstickcut, it's a thing - make it happen



Edited 1 time(s). Last edit at 10/12/2020 09:01AM by cKc.