Burnt Edges Are More Than Just Burnt

Posted by jasonstone20 
Burnt Edges Are More Than Just Burnt
March 08, 2019 12:39PM



Abrasive fatigue and impact fatigue are something you don't hear about often when it comes to damaged edges from the factory, mostly you just hear the term 'burnt edges'

------------------------------------------------------------------------------------------------------------------------------------------------------
"Gotta love living in 2019 baby, (63rc too soft on a production knife)"
--Shawn Houston

"I am still discussing issues of steels and performance at this stage."
--Cliff Stamp

"Cause geometry cuts, .....steel determines the level and the duration"
--Roman Landes

"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' "
--Sal Glesser
------------------------------------------------------------------------------------------------------------------------------------------------------
StoneSharpEdges
Re: Burnt Edges Are More Than Just Burnt
April 02, 2019 09:00PM
[www.bladeforums.com]

------------------------------------------------------------------------------------------------------------------------------------------------------
"Gotta love living in 2019 baby, (63rc too soft on a production knife)"
--Shawn Houston

"I am still discussing issues of steels and performance at this stage."
--Cliff Stamp

"Cause geometry cuts, .....steel determines the level and the duration"
--Roman Landes

"But in general, I'm all about high performance, Ergos, safety. That's why I've been accused of 'designing in the dark' "
--Sal Glesser
------------------------------------------------------------------------------------------------------------------------------------------------------
StoneSharpEdges
Sorry, only registered users may post in this forum.

Click here to login