If you are having issues with a finishing stone, whether C, M, F, or UF, try raising a burr on another stone and then removing the burr on the fine stone with a light edge leading pass progression like this: 10 on one side, 10 on the other, then 5, 5, 3, 3, 2, 2, 1, 1, alternating sides each time. The edge should catch hairs above the skin.