Sharpening carbides

Posted by sal 
This forum is currently read only. You can not log in or make any changes. This is a temporary situation.
sal
Sharpening carbides
January 16, 2021 02:30AM
One of our regulars on the Spyderco forum posted s question about whether or not we are sharpening the larger carbides or breaking them out. I though it was an interesting question that I too have thought about and I would guess many of you "Edge Junky"s" have thought of as well.

I would like to hear opinions on this, and I would especially respect to hear Cliff's thoughts on this?

sal
Re: Sharpening carbides
January 16, 2021 05:35PM
sal,
I guess it depends on the abrasives used and they type of carbide. Diamond and CBN should be able to cut any carbide, same with SiC.

"I am still discussing issues of steels and performance at this stage." -- Cliff Stamp, May his memory be a blessing
"Life is GOOD", -- Stefan_Wolf, May His Memory Be A Blessing
WordPress YouTube Facebook Patreon Locals Instagram Twitter
Re: Sharpening carbides
January 19, 2021 09:01AM
This link illustrates it quite wehll I think: [scienceofsharp.com]

So as Jason said it depends.